State about the prestressing steel, Civil Engineering

Assignment Help:

State about the Prestressing Steel

For prestressed concrete members, the high-tensile steel, used generally, consists of wires, bars or strands. The high tensile strength of steel is generally achieved by marginally increasing the carbon content in steel in comparison to mild steel. High-tensile steel usually contains 0.6 to 0.85% carbon, 0.7 to 1 % manganese, 0.05% of sulphur and phosphorus. The high carbon steel ingots are hot rolled into rods and cold drawn through a process of dies to reduce the diameter and increase the tensile strength. The durability of wires gets improved due to the cold-drawing operation. The cold-drawn wires are then tempered to improve their properties. Tempering or ageing or stress relieving by heat treatment of wires at 150-420°C improves the tensile strength. These cold-drawn wires are generally available in nominal sizes of 2.5, 3,4,5,7 and 8 mm diameter.  #question..


Related Discussions:- State about the prestressing steel

How to evaluate quality of bricks, Q. How to evaluate quality of Bricks? ...

Q. How to evaluate quality of Bricks? 1. Clour -Deep red, Carry red, Copper red, colour is indication of uniform burning and also suggests quality of clay used. Over brunt bric

Explain the allowable strength design (asd), Allowable Strength Design (ASD...

Allowable Strength Design (ASD) Process: - Apply service loads with no load factors - Assume linear elastic analysis of structure - Calculated stresses shall not excee

What is switch and expansion joint, Q. What is Switch and Expansion Joint? ...

Q. What is Switch and Expansion Joint? Switch Expansion, Joint (SEJ) is an expansion joint installed at each end of LWR/CWR to permit expansion/contraction of the adjoining bre

Raft and beam foundation, why is weight of raft not considered in structura...

why is weight of raft not considered in structural design of raft and beam

Define cast iron substructure - inspection of bridge, Define Cast iron subs...

Define Cast iron substructure - Inspection of bridge? Cast Iron also has the problem of corrosion due to atmosphere, which is similar to that of steel. However, in acidic or br

Define the frame column analysis, Define the Frame Column Analysis 1. B...

Define the Frame Column Analysis 1. Based on if a column section is a braced frame or unbraced frame. 2. Braced frame-indicates buckling mode shape does not involve tr

AERATED CONCRETE, AIR ENTRAINING AGENT USED IN CONCRETE OTHER THAN ALUMINIU...

AIR ENTRAINING AGENT USED IN CONCRETE OTHER THAN ALUMINIUM POWDER

Estimating, a 45 cm deep roof beam is provided on 30 cm wall of a room size...

a 45 cm deep roof beam is provided on 30 cm wall of a room size 3.0m*5.0m . calculate the quantity of steel required in beam on percentage basis.

Road drainage and maintenance, Road Drainage and Maintenance: The life...

Road Drainage and Maintenance: The life of a road depends upon how well and quickly the water is drained away from its various components. Similarly, regular and periodic insp

Write Your Message!

Captcha
Free Assignment Quote

Assured A++ Grade

Get guaranteed satisfaction & time on delivery in every assignment order you paid with us! We ensure premium quality solution document along with free turntin report!

All rights reserved! Copyrights ©2019-2020 ExpertsMind IT Educational Pvt Ltd