Planar defects

* Grain boundaries occur where the crystallographic direction of the lattice abruptly changes. This usually happens when two crystals start growing separately and then meet.

* Anti phase boundaries happen in ordered alloys: in this case, the crystallographic direction remains the same, every side of the boundary has an  opposite phase: For example if the ordering is usually ABABABAB, an anti phase boundary takes the form of ABABBABA.

 


Related Discussions:- Explain planar defects

Rheology, why do frosting on cakes do not fall off

why do frosting on cakes do not fall off

Heat exchanger, discuss the importence of heat exchanger in chemical proces...

discuss the importence of heat exchanger in chemical process

Want to know resin quantity, Hardness is 160 ppm and flow rate is 40 m3/hr ...

Hardness is 160 ppm and flow rate is 40 m3/hr ,I want to know the amount resin quantity required.Please give me a solution with details.

Heat capacity, Heat capacity: Heat capacity of furnace depend on (1)   ...

Heat capacity: Heat capacity of furnace depend on (1)         Thermal conductivity (2) Specific heat and (3) Specific gravity of refractory. The dense and heavy fire clay

Electostatic, merits and demerits of electrostatic sheilding.

merits and demerits of electrostatic sheilding.

Oil drop, what am i going to do nw

what am i going to do nw

Work, prove that work is a path function

prove that work is a path function

Write Your Message!

Captcha
Free Assignment Quote

Assured A++ Grade

Get guaranteed satisfaction & time on delivery in every assignment order you paid with us! We ensure premium quality solution document along with free turntin report!

All rights reserved! Copyrights ©2019-2020 ExpertsMind IT Educational Pvt Ltd