Planar defects

* Grain boundaries occur where the crystallographic direction of the lattice abruptly changes. This usually happens when two crystals start growing separately and then meet.

* Anti phase boundaries happen in ordered alloys: in this case, the crystallographic direction remains the same, every side of the boundary has an  opposite phase: For example if the ordering is usually ABABABAB, an anti phase boundary takes the form of ABABBABA.

 


Related Discussions:- Explain planar defects

Process engineering, 1. Select a process variable (pressure / temperat...

1. Select a process variable (pressure / temperature / level / flow) and conduct a literature survey to determine recent developments in process instrumentation field. Ide

#westron, #synthesis and uses of westron

#synthesis and uses of westron

Mass transfer operation, a. Explain the problems of flooding and channeling...

a. Explain the problems of flooding and channeling in packed tower

ASSIGHMENT, how nickel is incearing the toughness of steel?

how nickel is incearing the toughness of steel?

Perform an energy balance, Ammonia is oxidized with air to form nitric oxid...

Ammonia is oxidized with air to form nitric oxide in the first step to produce nitric acid.  The reaction occurs in a well insulated continuous reactor based on the stoichiometry:

Estimate the annual fugitive emission, Routine monitoring at a chemical pro...

Routine monitoring at a chemical process facility has detected fugitive emissions (leaks) of volatile organic compounds around several equipment valves, pump and compressor seals.

Write Your Message!

Captcha
Free Assignment Quote

Assured A++ Grade

Get guaranteed satisfaction & time on delivery in every assignment order you paid with us! We ensure premium quality solution document along with free turntin report!

All rights reserved! Copyrights ©2019-2020 ExpertsMind IT Educational Pvt Ltd