Planar defects

* Grain boundaries occur where the crystallographic direction of the lattice abruptly changes. This usually happens when two crystals start growing separately and then meet.

* Anti phase boundaries happen in ordered alloys: in this case, the crystallographic direction remains the same, every side of the boundary has an  opposite phase: For example if the ordering is usually ABABABAB, an anti phase boundary takes the form of ABABBABA.

 


Related Discussions:- Explain planar defects

Edta, how to find hardness of water by edta

how to find hardness of water by edta

Procedure classifying and handling of hazardous, ACTIVITY 1 to classify ha...

ACTIVITY 1 to classify hazardous chemicals based on the information given on the labels Requirements Bottles containing chemicals (generally used in a lab) = 20 in number.

1 Production of Chlorinated Polyvinyl Chloride, In the dryer air furnace, a...

In the dryer air furnace, a natural gas containing 92.5 mole% methane, 4.8% ethane, and the remainder propane is burned with 20% excess air. The fuel enters the furnace at 25°C and

Distribution Coefficient, theory behind the distribution of benzoic acid be...

theory behind the distribution of benzoic acid between water and benzene

Separation process, develop a process schematic which will yield separation...

develop a process schematic which will yield separation process streams

Write Your Message!

Captcha
Free Assignment Quote

Assured A++ Grade

Get guaranteed satisfaction & time on delivery in every assignment order you paid with us! We ensure premium quality solution document along with free turntin report!

All rights reserved! Copyrights ©2019-2020 ExpertsMind IT Educational Pvt Ltd