Planar defects

* Grain boundaries occur where the crystallographic direction of the lattice abruptly changes. This usually happens when two crystals start growing separately and then meet.

* Anti phase boundaries happen in ordered alloys: in this case, the crystallographic direction remains the same, every side of the boundary has an  opposite phase: For example if the ordering is usually ABABABAB, an anti phase boundary takes the form of ABABBABA.

 


Related Discussions:- Explain planar defects

Saponification number, Saponification number: Saponification number of oil...

Saponification number: Saponification number of oil is the number of milligram of potassium hydroxide required to saponify 1 g of oil. Mineral oils are the mixture of hydrocarbons

Water treatment, Ask question #haMinimum 100 words accepted#Okkkk Hardness ...

Ask question #haMinimum 100 words accepted#Okkkk Hardness of bore well water is less than sea water. Justify

Sds page, why only size influence the movement of protein in sds page

why only size influence the movement of protein in sds page

Rheology, why do frosting on cakes do not fall off

why do frosting on cakes do not fall off

Invitation of quotations-procedure, PROCEDURE:  Activity 1: Invitation of q...

PROCEDURE:  Activity 1: Invitation of quotations. A format for inviting a quotation is given below. You are required to fill up the form for finding out the prices of the follo

Explain the fluidized catalytic cracking method, 1. What are chemical fuels...

1. What are chemical fuels? How they are classified?  List the characteristics of a good fuel. 2. Define cracking. Explain the fluidized catalytic cracking method with neat diag

Hot lime soda process, the process of hot lime soda process for softening o...

the process of hot lime soda process for softening of water in detail

Gas law, a) The vacuum in the headspace of a can of food is normally forme...

a) The vacuum in the headspace of a can of food is normally formed by "hot fill" exhausting - that is, the cans are closed when the can is filled with product at a temperature o

Flooding and channeling in packed tower, Explain the problems of flooding a...

Explain the problems of flooding and channeling in packed tower

Write Your Message!

Captcha
Free Assignment Quote

Assured A++ Grade

Get guaranteed satisfaction & time on delivery in every assignment order you paid with us! We ensure premium quality solution document along with free turntin report!

All rights reserved! Copyrights ©2019-2020 ExpertsMind IT Educational Pvt Ltd