Planar defects

* Grain boundaries occur where the crystallographic direction of the lattice abruptly changes. This usually happens when two crystals start growing separately and then meet.

* Anti phase boundaries happen in ordered alloys: in this case, the crystallographic direction remains the same, every side of the boundary has an  opposite phase: For example if the ordering is usually ABABABAB, an anti phase boundary takes the form of ABABBABA.

 


Related Discussions:- Explain planar defects

Portland cement, describe layout of wet process for portland cement industr...

describe layout of wet process for portland cement industries ?

Water, what is break point on chlorination

what is break point on chlorination

Homework, Water from a supply having a total head of 100 ft is used in the ...

Water from a supply having a total head of 100 ft is used in the jet of an ejector in order to lift 10 ft3/s of water from another source (at a lower level) that has a total head o

Ro, what is the feed flow for a single memebrane

what is the feed flow for a single memebrane

.boiler trouble, how can be boiler trouble be minimised ?

how can be boiler trouble be minimised ?

Design project , hi, i am designing an (absorption column), i need help. ei...

hi, i am designing an (absorption column), i need help. either by a tutor to take me through the design, or by actually doing the design. please let me know if you help thanks

Corrosion ., the pilling bedworth ratio of iron is 1.77 why it not stable a...

the pilling bedworth ratio of iron is 1.77 why it not stable as per rulr

Write Your Message!

Captcha
Free Assignment Quote

Assured A++ Grade

Get guaranteed satisfaction & time on delivery in every assignment order you paid with us! We ensure premium quality solution document along with free turntin report!

All rights reserved! Copyrights ©2019-2020 ExpertsMind IT Educational Pvt Ltd