Planar defects

* Grain boundaries occur where the crystallographic direction of the lattice abruptly changes. This usually happens when two crystals start growing separately and then meet.

* Anti phase boundaries happen in ordered alloys: in this case, the crystallographic direction remains the same, every side of the boundary has an  opposite phase: For example if the ordering is usually ABABABAB, an anti phase boundary takes the form of ABABBABA.

 


Related Discussions:- Explain planar defects

Determine the void ratio, One cubic metre of wet soil weighs 19.80 kN. If t...

One cubic metre of wet soil weighs 19.80 kN. If the exact gravity of soil particles is 2.70 and water content is 11%, Determine the void ratio, dry density and degree of saturat

Pseudo order reactions, what are pseudo order reaction?with suitable exampl...

what are pseudo order reaction?with suitable example?

Malleability of a metal, Malleability of a metal is the Property by whi...

Malleability of a metal is the Property by which a material can be cold-worked

How are polymers classified, 1. a) How are Polymers classified?    b) De...

1. a) How are Polymers classified?    b) Define polymerization. Differentiate addition and condensation polymerization. 2. a) Explain the free radical mechanism of addition p

Polymers assignments, What are the applications of polymers in electrical a...

What are the applications of polymers in electrical and electronics industries>

Write Your Message!

Captcha
Free Assignment Quote

Assured A++ Grade

Get guaranteed satisfaction & time on delivery in every assignment order you paid with us! We ensure premium quality solution document along with free turntin report!

All rights reserved! Copyrights ©2019-2020 ExpertsMind IT Educational Pvt Ltd