Planar defects

* Grain boundaries occur where the crystallographic direction of the lattice abruptly changes. This usually happens when two crystals start growing separately and then meet.

* Anti phase boundaries happen in ordered alloys: in this case, the crystallographic direction remains the same, every side of the boundary has an  opposite phase: For example if the ordering is usually ABABABAB, an anti phase boundary takes the form of ABABBABA.

 


Related Discussions:- Explain planar defects

Concentrate a naoh solution , It is desired to concentrate a NaOH solution ...

It is desired to concentrate a NaOH solution from 12.5 % to 40% in a double effect evaporator. 50,000 lb/hr of feed solution enters the evaporator at 120 o F, and steam at 15 psig

Water, what is break point on chlorination

what is break point on chlorination

Procedure-design and infrastructure of a laboratory, PROCEDURE : Visit the...

PROCEDURE : Visit the preparation room of the lab (Physics/Chemistry/Zoology/I3otany), you studied in Exercise 1 and note its features. To make your study easy and to guide you, w

Order of reaction, on doubling the concentration of reactant,the rate of re...

on doubling the concentration of reactant,the rate of reaction triples.what is the order of reaction?

Titration, tell me everything about titration

tell me everything about titration

Chemical engineering thermodynamics 1, I want some lecture notes on propert...

I want some lecture notes on properties of pure substances, Ideal gas laws

Edta, edta softeninig numerical problems

edta softeninig numerical problems

Write Your Message!

Captcha
Free Assignment Quote

Assured A++ Grade

Get guaranteed satisfaction & time on delivery in every assignment order you paid with us! We ensure premium quality solution document along with free turntin report!

All rights reserved! Copyrights ©2019-2020 ExpertsMind IT Educational Pvt Ltd